Casting Metals
Melt and pour these alloys into molds to create metal parts and prototypes.
Lead-base coppered babbitt is able to withstand shock and vibration and requires less lubrication than other types of babbitt. Use it to cast bearings for low-speed, heavy-load applications.
Lead-Base Coppered Babbitt
Material Composition | Approximate | ||||||||||
---|---|---|---|---|---|---|---|---|---|---|---|
Melting Temperature, °F | Lead | Tin | Antimony | Copper | Arsenic | Thick. | Dia. | Wt., lbs. | Each | ||
625° | 75% | 10% | 14% | 0.3% | 0.5% | 1 1/2" | 3 3/4" | 4 1/2 | Rod and Disc | 0000000 | 0000000 |